The BFS/HL sorbent was prepared at a weight ratio of 30/70 with a slurrying time of 16h and a slurrying temperature of 65℃.
As a coal with bad slurrying property, Shenhua coal in Wushashan power Plant is pretreated by pyrolyzing in muffle and microwave pre-heating in nitrogen to improve its slurrying property.